The bromide problem can be seen on the negative as streaking marks, with 35mm film this can be seen round the sprocket holes.
Rodinal and HC110 are the most common developers used for semi-stand development. PyroCat HD (which we are trying at the moment) is another developer which can be used as a compensating developer.
I haven't used Rodinal but have used HC110 on many occasions.
With HC110, to get the compensating effect (reduce highlight density) use a more diluted solution and extend the development time.
HC110- Semi Stand
Add 1 stop to the initial exposure
I ALWAYS pre-soak the film for 5 minutes in water at roughly the same temperature as the developer. Since pre-soaking the film, I have not experienced and bromide drag (streaking marks on the film)
I use a dilution of 1:119 and develop the film for about 40 minutes with 4 gentle agitations at the 15 and 30 minute mark.
I use a water stop bath (this may reduce the life of the fixer)
I fix for 5 minutes or for( 9 minutes if using TMAX go remove the purple stain)
Rodinal and HC110 are the most common developers used for semi-stand development. PyroCat HD (which we are trying at the moment) is another developer which can be used as a compensating developer.
I haven't used Rodinal but have used HC110 on many occasions.
With HC110, to get the compensating effect (reduce highlight density) use a more diluted solution and extend the development time.
HC110- Semi Stand
Add 1 stop to the initial exposure
I ALWAYS pre-soak the film for 5 minutes in water at roughly the same temperature as the developer. Since pre-soaking the film, I have not experienced and bromide drag (streaking marks on the film)
I use a dilution of 1:119 and develop the film for about 40 minutes with 4 gentle agitations at the 15 and 30 minute mark.
I use a water stop bath (this may reduce the life of the fixer)
I fix for 5 minutes or for( 9 minutes if using TMAX go remove the purple stain)